Abstract
A resource and energy saving technology for obtaining white cement has been developed. It has been shown that the introduction of 10% phosphoangihydrate and 20-30% clay and up to 20% sulfoxlicer increases the whiteness of white cement, the degree of which reaches 85% by BaSO4 and converts the mixed white cement into a cement with normal setting time.