The goal is to reduce the sintering temperature of ceramics based on zinc orthostannate. This can be done by introducing sintering additives, which are manganese and nickel oxides. During the synthesis of zinc orthostannate, substitutional solid solutions are formed, which make it possible to activate the sintering process, create a denser structure of the final product, while special chemical methods for preparing powders make it possible to reduce the temperature of solid solution synthesis and ceramic sintering by at least 100 °С.